Atomic Layer Deposition (ALD) is a thin film deposition technique that operates based on a self-limiting and sequential process. ALD enables precise control over film thickness, composition, and uniformity at the atomic scale. Understanding the step-by-step process of ALD provides insight into how this technique works.
1. Substrate Preparation:
Before the deposition process begins, the substrate surface is carefully prepared. It is typically cleaned to remove contaminants and oxides, ensuring a clean and reactive surface for the ALD process.
2. Precursor Introduction:
The ALD process starts by introducing the first precursor into the reaction chamber. The precursor can be in the form of a gas or a volatile liquid. It is chosen based on its reactivity with the substrate surface and the desired film material.
3. Adsorption:
The first precursor molecules are introduced into the reaction chamber, where they adsorb onto the substrate surface. The adsorption occurs due to chemical reactions or weak physical forces, such as van der Waals interactions, depending on the specific precursor and substrate combination.
4. Purge/Flush:
After a sufficient adsorption time, the excess or unreacted precursor is removed from the chamber. This step is typically achieved by purging or flushing the chamber with an inert gas, such as nitrogen, to eliminate any residual precursor molecules.
5. Reaction with the Second Precursor:
Once the substrate surface is purged, the second precursor is introduced into the chamber. This precursor reacts selectively with the adsorbed precursor on the surface, forming a new layer on top of the initial monolayer. The reaction is designed to be self-limiting, allowing only one layer to form during each deposition cycle.
6. Purge/Flush:
Similar to the first precursor, the excess or unreacted second precursor is removed by purging or flushing the chamber with an inert gas. This step ensures that only the desired reactants remain on the surface.
7. Repeat Cycle:
The above steps are repeated for the desired number of cycles, allowing for the controlled growth of the thin film layer by layer. Each cycle adds one atomic layer to the film, resulting in precise control over the film thickness.
8. Monitoring and Control:
During the ALD process, monitoring and control techniques are employed to ensure accurate deposition and film quality. In situ monitoring techniques, such as spectroscopy or ellipsometry, provide real-time information about film thickness, composition, and properties. This information enables adjustments and optimizations to achieve the desired film characteristics.

9. Film Properties and Applications:
The resulting ALD-deposited thin film exhibits excellent conformality, uniformity, and atomic-level control. These properties make ALD highly valuable in various applications, including semiconductor devices, energy storage systems, catalysis, coatings, and more.
Atomic Layer Deposition (ALD) works through a sequential and self-limiting process, allowing precise control over film growth at the atomic scale. By carefully selecting and alternating precursors, adsorption, reaction, and purge/flush steps, ALD enables the deposition of thin films with tailored thickness, composition, and properties. The ability to achieve atomic-level control makes ALD a versatile technique with applications in a wide range of industries and research fields.